Breakages during Heat sock test

I have serious problems with HST, because all my glass plates break during the process (every 100 plates 80 are broken). The plates are 1500 x 2500 mm, glass tickness is 12 mm, the holes are D=12mm and are 24mm distant from the long sides. There are total 8 holes. At the corners the holes are 160mm and 30mm distant (from the edges). During the tempering process all is OK. In the HST process during the cooling phase the glass break.

I don't know if the problem is the tempering process or maybe the position and the diameter of the holes.What do you suggest me?

Low E Glass in Single Glazing

I am a developer in India and making a huge commercial project of 1 million sqft. We want to use hard coated low e glass in single glazing. Ours is a dry and hot climate, where temperature varies from 35 to 45 degrees most time of the year. Can we use low e glass in single glazing and will it give the required performance in single glazing ?

"dual method"

There are two method of installing tempered glass for shower screen.There is with aluminium "u"channel embedded into concrete floor and one without but with groove line space by the tiles to recieved the glass.As shower cubicle is a wet area,Which method is practise throughout without affecting the edge of the glass to concrete surface.